Toner + water + peach gum without transparent glaze renderings
Usage: 1. Toner+water+peach gum
2. First, the toner is mainly used as underglaze paint. After buying various colors, add tea water (blue and white materials) or water to paint on the dried body, and then spray transparent glaze to burn various patterns.
Second, because the firing temperature of color powder is very wide, it can be fired from 1200 to 1320 degrees, so it is also an excellent pigment that we add to the glaze. When color powder of various colors is added to the transparent glaze, it can become glaze of various colors, and the effect is very obvious.
Third: The toner can be added to the mud to turn it into colored mud of various colors. We just need to directly shape the colored mud and spray a layer of transparent glaze to burn it. The effect is very beautiful.
¡Ø Warm tips on color
1. The toner is taken in kind. Due to different light, display and other objective reasons, or some color difference, please take the received material object as the standard
2. Parents with strict requirements on hair color effect can make a test piece before firing to ensure that the color is what they want and then use it in large quantities. Different furnaces, different temperatures, different placement environments, different glaze thickness, and different clay will affect the color of the pigments.
![](https://ae01.alicdn.com/kf/S882995337c884ee6bcf6b8b5428f020fj.jpg?width=532&height=3348&hash=3880)
![](https://ae01.alicdn.com/kf/S3e85254cfaa5499d98be5ce6312ee1e3d.jpg?width=532&height=3500&hash=4032)
![](https://ae01.alicdn.com/kf/Sf4c7fe9951c74342af72895e6d5aaf5cz.jpg?width=532&height=4234&hash=4766)
Color modulation steps
1. Preparation materials: toner, tea, peach gum, sponge ball, small dish, brush.
2. Pour out a certain amount of toner and mix it evenly in the proportion of 1:3 water and toner
3. Add 10% peach gum to make the color better adhere to the green body and not easy to fall off
4. Wipe the green body with a small sponge to moisturize (replenish water), and then you can start painting on the green body. After painting, put it in the kiln to burn, and you can see your creation![](https://ae01.alicdn.com/kf/Scc7ee66eb8c14e8581eed0c7c0bc6633M.jpg)
Color glaze
1. The proportion of monochrome powder, polychrome powder and basic glaze (can be transparent glaze and matte white glaze) is 10~3% by weight respectively (Light color) 4% - 7% (medium color glaze more than 8% (dark color glaze)
2. When adding basic glaze, try to pass 160 mesh sieve and absorb iron,
3. Pycnometer for customers with high requirements. Glue glaze is about 45 specific gravity, Baume degree is 46, spray glaze is 50 specific gravity, Baume degree is 1.5, each type of different glaze will be a little different, only by trial firing can we find the best glaze performance, and the glaze effect of pottery can be guaranteed![](https://ae01.alicdn.com/kf/S78b91e59188d4d73bed866fb483aba73K.jpg)
Handmade mud
(The proportion of color powder and mud is 1%~3% of the weight of the electric kiln respectively. Add 2-3% to the gas kiln. 2. Soak the mud in water and mix it evenly to form mud. 3. Add a small amount of color powder, put it on the gypsum board after the mud is mixed evenly, and knead it to shape when the water is dry (about 50g~100g can adjust 1.5kg mud)![](https://ae01.alicdn.com/kf/S3cb53968ae5a4e2abbbbf12d2016ddba7.jpg)
Product live shot display
![](https://ae01.alicdn.com/kf/S72ccdd9e370c4192bba99964be1b08ecS.jpg)